MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Geon® Performance Solutions Vinyl Flexible A5500  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Transparent

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.027 - 0.031 cm/cm0.027 - 0.031 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5555ASTM D2240
 50
@Time 15.0 sec
50
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 7.58 MPa1100 psi510 mm/min; ASTM D638
Tensile Stress at Strain 2.76 MPa
@Strain 100 %
400 psi
@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 440 %440 %510 mm/min; ASTM D638
Tear Strength 31.5 kN/m180 pliDie C, 510 mm/min; ASTM D624
Compression Set 20 %
@Temperature 23.0 °C,
Time 79200 sec
20 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus  0.00689 GPa
@Temperature 23.0 °C
0.999 ksi
@Temperature 73.4 °F
ASTM D1043
 0.310 GPa
@Temperature -58.0 °C
45.0 ksi
@Temperature -72.4 °F
ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -57.8 °C-72.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 3.0 %
@Thickness 1.90 mm
3.0 %
@Thickness 0.0748 in
ASTM D1003
Transmission, Visible 85 %
@Thickness 1.90 mm
85 %
@Thickness 0.0748 in
CIE Illuminant C; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 166 °C320 - 331 °F
 188 - 199 °C370 - 390 °F
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGeneral Purpose
 High Gloss
FormsPellets
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AlphaGary PVC GM 8000-95C Natural LCF Polyvinyl Chloride Thermoplastic

PH1PN8348 / 102184

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.