MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Dover Chemical DOVERPHOS 4HR PLUS Trisnonylphenyl Phosphite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos 4HR PLUS is trisnonylphenyl phosphite (TNPP) with approximately 1.00% triisopropanolamine. It is an aryl phosphite with a high molecular weight and low phosphorus content. It is an effective liquid phosphite heat stabilizer for a wide variety of applications, including: polyolefin, acrylics, adhesives, elastomers, nylon, polycarbonate, polyurethanes, polystyrene, PVC, coatings, ABS, and polyethylene terephthalate. Typical use levels range from 0.05 to 3.00% for most applications.

Information provided by DoverChem

Key Words: CAS# 26523-78-4/122-20-3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 - 0.992 g/cc
@Temperature 25.0 °C
0.980 - 0.992 g/cc
@Temperature 77.0 °F
ASTM D1298
Density 0.983 g/cc0.0355 lb/in³
Viscosity 5900 cP
@Temperature 25.0 °C
5900 cP
@Temperature 77.0 °F
Molecular Weight 688 g/mol688 g/mol
ASTM Color <= 75<= 75APHA; ASTM D1209
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.30<= 0.30[mgKOH/gm]; ASTM D3242
 
Optical PropertiesMetricEnglishComments
Refractive Index <= 1.528
@Temperature 25.0 °C
<= 1.528
@Temperature 77.0 °F
ASTM D1218
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 4.3 %4.3 %
 
Descriptive Properties
AppearanceClear liquid
NP, %<4Free Nonylphenol, DP260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER027 / 217646

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.