MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Matexcel NAT-0017 Collagen Type I solution from rat tail
Categories: Wood and Natural Products

Material Notes: Col1a1 (Collagen, type I, a1) or Collagen is a major structural human protein, which assembles in the form of fibrils. It is a very long, thin and the most abundant protein found in the human body. It is a supercoiled right-helix of three left-handed polypeptide chains. These chains are composed of ~1040 amino acids, which are essentially repeats of three amino acids -(Gly-X-Y)n. Gly is glycine and X and Y can be any amino acids, but in humans are usually proline and hydroxyproline, respectively. Collagen is an essential ingredient of connective tissue. Studies in a Chinese family show that mutation in COL1A1 (Collagenase type I) is linked with type I osteogenesis imperfecta. Collagen is linked with subchondral turnover of bone, and might have potential as marker to determine the state of joint space narrowing and osteophytes in osteoarthritis.

Application: Used as a coating material to support adherent cells growth and differentiation.

Morphology: powder

Uses: Recommended for use as a cell culture substratum. May not be suitable for 3-D gel formation. Sterile solution prepared from rat tail tendons by a modification of the published extraction method 1. It is supplied as an aqueous solution in 20mM acetic acid with a protein concentration as stated on the bottle. (approx.100mg protein per vial). Protein concentration was estimated by the Biuret method 2. SDS polyacrylamide gel electrophoresis analysis shows the typical band pattern for Type I Collagen, with a doublet at apparent molecular weights of 115 and 130kDa and another doublet at 215 and 235kDa. Based on this analysis, the purity of the Collagen sample is >95%.

Key Words: Synonyms: Collagen; Source: rat tail
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Storage Temperature 2.00 - 8.00 °C35.6 - 46.4 °F
 
Descriptive Properties
impuritiesEndotoxin: <0.25 EU/Ml
Shipping & PackagingApprox. 100mg/vial (Volume 22 - 25ml/vial, see label for lot-specific protein concentration)
Stabilitysuitable for cell culture
Surface coverage6-10 µg/cm2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1016 / 299647

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.