MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Medalist® MD-53278 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-53200 series is a high performance thermoplastic elastomer series, designed to be a sustainable alternative to flexible PVC for medical tubing and film. Medalist MD-53278 is a medium hardness, low density, clear, lubricated grade, available in Nat and color-matched, intended for use in medical and healthcare applications, with excellent processability and throughput in extruded tubing.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Melt Strength; Good Processability; Good Toughness; Halogen Free; High Clarity; Medium Hardness; High Purity; Kink Resistant; Low Density; Low Specific Gravity; Lubricated; No Animal Derived Components; Radiation (Gamma) Resistant

Uses: Clear Sheet; Film; Hose; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Tubing

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Cast Film; Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 7.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
7.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  79
@Time 5.00 sec
79
@Time 0.00139 hour
ASTM D2240
 81
@Time 1.00 sec
81
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 15.0 MPa2170 psiASTM D412
Tensile Stress at Strain  4.45 MPa
@Strain 50 %
645 psi
@Strain 50 %
ASTM D412
 4.79 MPa
@Strain 100 %
695 psi
@Strain 100 %
ASTM D412
 6.76 MPa
@Strain 300 %
980 psi
@Strain 300 %
ASTM D412
Elongation at Break 620 %620 %ASTM D412
Tear Strength 64.3 kN/m367 pliASTM D624
Compression Set  23 %
@Temperature 22.8 °C,
Time 79200 sec
23 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 83 %
@Temperature 70.0 °C,
Time 79200 sec
83 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 227 °C380 - 440 °FMelt, Injection
Rear Barrel Temperature 149 - 171 °C300 - 340 °FInjection
Middle Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Front Barrel Temperature 193 - 227 °C380 - 440 °FInjection
Nozzle Temperature 193 - 227 °C380 - 440 °FInjection
Zone 1 160 - 188 °C320 - 370 °FExtrusion
Zone 2 182 - 196 °C360 - 385 °FExtrusion
Zone 3 182 - 204 °C360 - 400 °FExtrusion
Zone 4 182 - 204 °C360 - 400 °FExtrusion
Zone 5 182 - 210 °C360 - 410 °FExtrusion
Die Temperature 177 - 216 °C350 - 420 °FExtrusion
Mold Temperature 21.1 - 51.7 °C70.0 - 125 °FInjection
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psiInjection
Cushion 0.356 - 2.54 cm0.140 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0747 / 237238

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.