MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Polymer Industries Densetec HDPE Pipe Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It retains its properties between 220°F and 180°F, and resists most chemicals. It is also NSF certified under Standard 61 to be used in potable water piping systems.

Information provided by Polymer Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D1505
High Load Melt Index 11 g/10 min
@Load 21.6 kg,
Temperature 190 °C
11 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 100 hour>= 100 hourSlow Crack Growth; ASTM F1473
Tensile Strength, Yield 22.0 MPa3190 psi2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break 800 %800 %2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 0.960 GPa139 ksiTangent; ASTM D790
 0.760 GPa
@Strain 2 %
110 ksi
@Strain 2 %
Secant; ASTM D3350
Hydrostatic Design Basis 5.50 MPa798 psi140°F; ASTM D2837
 11.0 MPa
@Temperature 23.0 °C
1600 psi
@Temperature 73.4 °F
ASTM D2837
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polymer Industries Densetec HDPE Sheet
Ineos K38-20-123 Pipe Extrusion Grade Polyethylene
Formosa Plastics Formolene® HP6000 Pipe HDPE
Formosa Plastics Formolene® HP4401 Pipe HDPE
Formosa Plastics Formolene® HP4000 Pipe HDPE

PPOLIND07 / 56983

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.