MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BASF Ultramid® STAR S 216 V30 NATURAL Nylon 6, 30% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Product Description: Ultramid® STAR S 216 V30 NATURAL is based on a patented high flow polyamide 6 resin, reinforced with 30% of glass fiber, for injection molding. Due to its outstanding flow characteristics, this grade provides a significant productivity improvement and allows more freedom in mold and part design versus a standard polyamide solutions.

Availability: Africa & Middle East; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Features: Good Mold Release; High Flow; Outstanding Surface Finish

Uses: Consumer Applications; Furniture; General Purpose; Industrial Applications; Outdoor Applications; Power/Other Tools

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Natural Color; Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Maximum Moisture Content 0.20
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16000 psiISO 527-2
Tensile Modulus 899000 psiISO 527-1
Flexural Modulus 754000 psiISO 178
Izod Impact, Notched (ISO) 9.00 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) 31.0 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 43.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 6.70 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+12 ohmIEC 62631-3-2
Dielectric Constant 4.5
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 560 V/mil
@Thickness 2.00 mm
IEC 60243-1
Dissipation Factor 0.090
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 475 VSolution A; IEC 60112
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 446 - 455 °F
Middle Barrel Temperature 455 - 464 °F
Front Barrel Temperature 464 - 473 °F
Mold Temperature 140 - 194 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2049 / 310742

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.