MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Zircar Ceramics Alumina Furnaceware
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: ZIRCAR Ceramics Alumina Furnaceware are high purity fully dense, fine grain aluminum oxide products suitable for use in applications with temperatures as high as 1800°C. Such uses include crucibles for crystal growth or glass melting, process tubes, and inert high temperature supports and fixturing. Available as crucibles, tubes, rods, and special geometries.

Information provided by Zircar Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.91 g/cc0.141 lb/in³
Open Porosity 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 380 MPa55100 psi
 165 MPa
@Temperature 1000 °C
23900 psi
@Temperature 1830 °F
Compressive Strength 3650 MPa
@Temperature 20.0 °C
529000 psi
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.40 µm/m-°C
@Temperature 20.0 - 1000 °C
4.67 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity  8.20 W/m-K
@Temperature 800 °C
56.9 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 36.0 W/m-K
@Temperature 20.0 °C
250 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1800 °C3270 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99.82 %99.82 %
B2O3 0.0010 %0.0010 %
CaO 0.040 %0.040 %
Cr2O3 0.0030 %0.0030 %
Fe2O3 0.025 %0.025 %
K2O 0.0010 %0.0010 %
MgO 0.035 %0.035 %
Na2O 0.0080 %0.0080 %
SiO2 0.060 %0.060 %
TiO2 0.0040 %0.0040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CZIR000 / 2808

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.