MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Poco Graphite Premium Graphite Glass Handling Graphite Grade CXT-X Graphite
Categories: Carbon; Graphite

Material Notes: CXT-X graphite is the ideal material for bulkier parts in the glass handling process. CXT-X graphite is an economical material used for larger parts in the glass handling process. Features: Average particle size of less than 20 microns provides moderate strength. Better wear resistance than traditional materials, decreases downtime due to replacements or breakage. Our graphite grades are available as semi-finished rods, blocks, plates, and fully machined parts. Applications: Lehr stacker pads. Fabrication of large glass-handling parts. Applications not requiring high material strength.

Information provided by Entegris POCO Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/cc
Particle Size <= 20 µm
Ash <= 0.30 %< 3000 ppm ash
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71
Flexural Strength 9800 psiMeasured using three-point bend method.
Compressive Strength 15900 psi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.80 µm/m-°C
Thermal Conductivity 85.0 W/m-KRoom temperature; as temperature increases, thermal conductivity decreases.
Maximum Service Temperature, Air 450 °COxidation threshold; weight loss after 24 hours is about 1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CPOCO405 / 268790

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.