This concentrate has been developed for blending with polyolefin resins intended for conduit pipe applications. The carrier resin was selected for maximum compatibility with HDPE grades used in pipe conduit extrusion. Description/Features: Applications: Market: Note: 2882EL Grey PEC contains a hindered amine light stabilizer to provide three years protection against ultraviolet light exposure, and has been ideally formulated to allow for a 4% letdown. Information provided by PolyOne Corporation. |