MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Morgan Advanced Ceramics Pyro-Bloc® Y Modules ZR Grade Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: The Pyro-Bloc Y and Y2 modules are manufactured from a high purity blend of raw materials which are used to produce R Grade (alumina-silica), ZR Grade (alumina-zirco-nia-silica), and C Grade (alumina-silica-chromia) ceramic fibers. The modules utilize a specially designed 316 stainless steel internal support system and industry standard Pyro-Bloc stud system. In addition, it has no hot face, cold face, or side constrictions which permit maximum module- to-module compression and easily conforms to irregular steel shell surfaces during installation. The modules use the proven center-fire, one-step weld system which eliminates the need for pre-laid out stud patterns.

Applications:

  • Annealing furnaces
  • Heat treating furnaces
  • Process heaters
  • Reformers
  • Ethylene furnaces
  • Forge furnaces
  • Steam flood units
  • Homogenizing furnaces
  • Incinerators

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.160 g/cc0.00578 lb/in³
 0.192 g/cc0.00694 lb/in³
 0.240 g/cc0.00867 lb/in³
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0700 W/m-K
@Temperature 260 °C
0.486 BTU-in/hr-ft²-°F
@Temperature 500 °F
at 160 kg/m3; ASTM C-201
 0.150 W/m-K
@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1000 °F
at 160 kg/m3; ASTM C-201
 0.260 W/m-K
@Temperature 816 °C
1.80 BTU-in/hr-ft²-°F
@Temperature 1500 °F
at 160 kg/m3; ASTM C-201
 0.390 W/m-K
@Temperature 1093 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 1999 °F
at 160 kg/m3; ASTM C-201
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air <= 1343 °C<= 2449 °F
 <= 1427 °C<= 2601 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 <= 37.5 %<= 37.5 %
SiO2 47 %47 %
ZrO2 15.5 %15.5 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel
Yttria Stabilized Zirconia, YSZ
X5CrNiMo1713 Austenitic stainless steel for medical instruments
205 Austenitic Stainless Steel (UNS S20500)

CMORF6468 / 203252

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.