VESTAKEEP® 5000 FP is an unreinforced, high viscosity polyether ether ketone fine powder. It can be used as a basic resin or in blends with different additives for manufacturing compression molding parts. The semi-crystalline polymer features superior, thermal and chemical resistance. VESTAKEEP® 5000 FP is of low flammability. VESTAKEEP® 5000 FP is supplied as powder in 10 kg boxes with moisture-proof polyethylene liners. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. For information about processing of VESTAKEEP® 5000 FP, please follow the general recommendations in our brochure “VESTAKEEP® High Performance in Powder Form Polyether Ether Ketone Powders“. Pigmentation may affect values. Dry properties listed below Industrial Sector: Automotive and Mobility, Aircraft and Aerospace Processing: Press and sintering Delivery form: Powder Resistance to: Heat (thermal stability), Fire / burn Applications: Electrical and Electronical Processing: Electrostatic coating Special Characteristics: High viscosity Color: Natural color Delivery form: Fine powder (FP) Chemical Resistance: General chemical resistanceInformation provided by Evonik. |