MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Armacell Armafix® Insulation Pipe Hanger
Categories: Other Engineering Material

Material Notes: The quick, innovative Insulation Pipe Hanger (IPH) alternatives to traditional block and dowel pipe supports
  • Engineered from Armaflex (IPH) insulation
  • Closed cell structure for total system integrity
  • Single-piece construction, self-adhesive closure, exclusive foam-to-foam bond
  • Quick and easy 3-step installation
  • Armafix IPH: 3/4" and 1" wall sizes (also 1/2" wall –special order), ID range from 3/8" ID to 8" IPS
See manufacture for sizes

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 - 0.176 g/cc0.00463 - 0.00637 lb/in³ASTM D1622 or D1667
Water Absorption 0.20 %0.20 %ASTM C209
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.0360 W/m-K
@Temperature 24.0 °C
0.250 BTU-in/hr-ft²-°F
@Temperature 75.2 °F
ASTM C177 or C518
 0.0370 W/m-K
@Temperature 32.0 °C
0.257 BTU-in/hr-ft²-°F
@Temperature 89.6 °F
ASTM C177 or C518
Maximum Service Temperature, Air 105 °C221 °FASTM C534
Minimum Service Temperature, Air -183 °C-297 °FASTM C534
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
Water Vapor Permeability0.05 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell NH Armaflex® Nonhalogen insulation in flexible tubes, sheets and rolls
Armacell Armaflex® COIL Tube Insulation
Armacell Armaflex® 520 Adhesive
Armacell AP Armaflex® SA Through 1" Self-Adhering Sheet & Roll Insulation
Armacell AP Armaflex® SA 1 1/2" & 2" Self-Adhering Sheet & Roll Insulation

PARMD022 / 186633

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.