Amco Amalloy® B1172 Polymer Alloy
(discontinued **)
Categories:
Polymer
;
Thermoplastic
Material Notes:
Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.
Impact modified, very clear, moderate flow.
Information provided by Amco Plastic Materials.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Melt Flow
2.7
g/10 min
@Load 3.80 kg,
Temperature 230 °C
2.7
g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
32.8
MPa
4750
psi
ASTM D638
Tensile Strength, Yield
35.2
MPa
5100
psi
ASTM D638
Elongation at Break
52 %
52 %
ASTM D638
Tensile Modulus
2.76
GPa
400
ksi
ASTM D638
Flexural Strength
66.9
MPa
9700
psi
ASTM D638
Flexural Modulus
2.69
GPa
390
ksi
ASTM D790
Izod Impact, Notched
0.534
J/cm
@Thickness 6.35 mm,
Temperature 22.8 °C
1.00
ft-lb/in
@Thickness 0.250 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Vicat Softening Point
98.9
°C
210
°F
ASTM D1525
Optical Properties
Metric
English
Comments
Haze
3.1 %
3.1 %
ASTM D1003
Transmission, Visible
91.6 %
91.6 %
ASTM D1003
**
Materials flagged as discontinued (
) are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.
Users of our Advanced Search (registration required) may exclude discontinued materials from search results.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Amco Amalloy® B9714 Polymer Alloy
PMCO09 / 52494
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.