LD 103 resins are homopolymer industrial film resins with excellent toughness. LD 103 resins have a low melt index, which provides good impact strength and melt strength over a range of gauges. Availability: Latin America, North America. Additive: antiblock: no; slip: no; thermal stabilizer: yes. Applications: agricultural film, form fill and seal packaging, medium duty shrink film, blend partner, freezer film, rubber bale wrap, co-extrusion films, liners. Forms: pellets. Information provided by ExxonMobil. |