MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ DP620NS Structural Adhesive
Categories: Polymer; Adhesive

Material Notes: 3M™ Scotch-Weld™ Urethane Adhesive DP-620NS is a back, long working time, two-component polyurethane. Formulated as 1:1 ratio liquids. With the squeeze of the trigger, or with automated dispensing the components are automatically mixed and dispensed through a static mixer tip as a bubble-free, non-sag paste. At room temperature the mixture will set within 4 hrs and fully cure in 48 hours at room temperature. Cure can be accelerated with heat.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 17.2 MPa2500 psiASTM D1002-72
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.0 °C-59.8 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min4.00 hourTime to Handling Strength
 2880 min48.0 hourFull Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
Solvay LTM® 26EL Epoxy with 34-700 Unidirectional Carbon Laminate Prepreg
Solvay CYCOM® 2020 Epoxy + T800-6K 2X2T Twill 200 Prepreg, without Post-Cure

PMM34661 / 169408

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.