Total Petrochemicals Polystyrene 818 is a high heat resistant, high impact Polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacturing of articles which require good dimensional stability at elevated temperatures. Suitable Applications for Total Petrochemicals Polystyrene 818 include TV covers, printers, scanners, electrical appliances. Information provided by Total Petrochemicals. |