MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NOVA Chemicals SURPASS® PF-Y818-CPX Butene Copolymer LLDPE Film Resins
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Features: moderate toughness, superior melt strength for high output film lines, blends well with LDPE. Common Additives: processing stabilizer, AB (2500ppm), PPA.

Applications: food packaging, industrial packaging, liners.

Film properties reported are typical of blown film extruded on a 2.5" extruder with 4" die and 100-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.919 g/cc0.0332 lb/in³ASTM D 792
Thickness 25.0 microns0.984 milAs tested
Melt Index of Compound 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Antiblock Level 2500 ppm2500 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.0 MPa1450 psiASTM D882
Film Tensile Strength at Yield, TD 11.0 MPa1600 psiASTM D882
Film Elongation at Break, MD 500 %500 %ASTM D882
Film Elongation at Break, TD 810 %810 %ASTM D882
Elmendorf Tear Strength MD 50 g
@Thickness 0.0250 mm
50 g
@Thickness 0.000984 in
ASTM D1922
Elmendorf Tear Strength TD 475 g
@Thickness 0.0250 mm
475 g
@Thickness 0.000984 in
ASTM D1922
Dart Drop Test 115 g
@Thickness 0.0250 mm
0.254 lb
@Thickness 0.000984 in
ASTM D1709/A
Film Tensile Strength at Break, MD 47.0 MPa6820 psiASTM D882
Film Tensile Strength at Break, TD 33.0 MPa4790 psiASTM D882
1% Secant Modulus, MD 175 MPa25400 psiASTM D882
1% Secant Modulus, TD 230 MPa33400 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %
@Thickness 0.0250 mm
7.0 %
@Thickness 0.000984 in
ASTM D1003
Gloss 65 %
@Thickness 0.0250 mm
65 %
@Thickness 0.000984 in
ASTM D2457
 
Descriptive Properties
Low Friction Puncture84 J/mmNOVA Chemicals test

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOV609 / 249056

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.