MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CMW® ELKONIUM 41 palladium based alloy  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: This material has been rebranded as a part of the NAECO® ELKONIUM® product line.

Palladium belongs to the platinum group of metals and like platinum is highly resistant to atmospheric corrosion; however, it begins to tarnish at temperatures above 400(C. It has a high melting point (1552(C) and, like platinum, resists arc formation. Its low electrical conductivity (16% IACS) limits its application to low current circuits. It costs much less than platinum, and is used as a lower cost alternative. Economics normally dictate that it be supplied as a composite contact with a thin contact metal facing silver brazed to a nickel-plated steel rivet, screw, or projection weld button backing.

ELKONIUM® 41 is a palladium-silver-nickel alloy sold by CMW, which is tarnish resistant and considerably harder than pure palladium. It is one of the more economical precious metals and is used in business machines where the contacts operate at high repetitive rates and close with impact. A contact combination very resistant to metal transfer and sticking is obtained when ELKONIUM 41 alloy is operated against a tungsten negative contact,

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.5 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 15T 82annealed
 90cold worked
Tensile Strength, Ultimate 68000 psiannealed
 100000 psicold worked
Elongation at Break 2.0 %cold worked
 13 %annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000430 ohm-cm4 % IACS
 
Component Elements PropertiesOriginal ValueComments
Nickel, Ni 2.0 %
Palladium, Pd 72 %
Silver, Ag 26 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NAECO® ELKONIUM® 28 Silver Alloy
CMW® ELKONIUM 28 Silver Alloy

NCMW107 / 15923

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.