MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuBois Parquench 60 Water-Based Quenchant
Categories: Fluid; Quenchant

Material Notes: The lower molecular weight polymer package. It is generally used for lower alloy steels, castings, forgings and most aluminum applications. Typical concentration is 15%.

Information provided by Heatbath Corporation - Park Metallurgical.

Heatbath/Park has been acquired by DuBois Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 30 SUS
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °FUpper limit of working range
Minimum Service Temperature, Air 80.0 °FLower limit of working range

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, Alpha SiC
Thermal Transfer Composites PRIMEX™ MCX724™ Aluminum Silicon Carbide Composite, Reinforced
Silicon Carbide, Reaction-Bonded, SiSiC
Silicon Carbide, CVD
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide

WHEATB19 / 75974

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.