MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Indorama StarPet Preformance® N2R PET Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: PREFORMANCE® PET N2R is a food grade PET copolymer specially designed for the water container market. It offers excellent clarity and color and a low acetaldehyde content to help minimize impact on aroma and flavor. It offers enhanced reheat ability that improves machine efficiency during blow molding.

PREFORMANCE® PET N2R resin is considered safe for food packaging applications based upon compliance with FDA Regulation 21 CFR Section 177.1630 and USP 661 specifications.

Key Words: Enhanced reheat ability
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.897 g/cc0.0324 lb/in³QSWI 8.2.4.150
Viscosity Test 74 - 78 cm³/g0.74 - 0.78 dl/gIntrinsic; QSWI 8.2.4.101
 
Chemical PropertiesMetricEnglishComments
Acetaldehyde <= 1.00 ppm<= 1.00 ppmQSWI 8.2.4.114
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %as packed, QSWI 8.2.4.112
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Color, CIE79.5 to 84.5 (L)QSWI 8.2.4.104
Contaminants/Black SpecsNone
Dust<300 ppmas packed, QSWI 8.2.4.132
ProcessBlow Molding
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Indorama Auriga Polymers Polyclear™ Refresh 1101 PET Resin
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Indorama StarPet Preformance® 1708 PET Resin
DAK Americas Laser+® W L40A PET
Iran Petrochemical (PCC) PET BG-800 Polyethylene Terephthalate

PINDOC916 / 126599

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.