MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hapco TUFFALLOY 4272 High Strength Urethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: TUFFALLOY 4270 is a series of Liquid Molding Compounds with thermoplastic properties such as high impact, high heat distortion, and low viscosity. This unique chemistry developed by Hapco to meet today’s market demands for prototype and low production parts needs.

KEY ADVANTAGES:

  • Fast Cycle Time
  • Excellent Physical Properties
  • Low Viscosity
  • 1:1 Mix Ratio
TUFFALLOY 4270 Series is available in two speeds.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D-4669
Viscosity 250 - 350 cP250 - 350 cPASTM D-4878
Linear Mold Shrinkage 0.0010 - 0.0040 cm/cm0.0010 - 0.0040 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 79 - 8979 - 89ASTM D-2240
Tensile Strength 84.8 MPa12300 psiASTM D-638
Elongation at Break 7.0 %7.0 %ASTM D-638
Modulus of Elasticity 2.82 GPa409 ksiASTM D-638
Flexural Strength 98.6 MPa14300 psiASTM D-790
Flexural Modulus 2.85 GPa414 ksiASTM D-790
Izod Impact, Notched 0.801 J/cm1.50 ft-lb/inASTM D-256
Izod Impact, Unnotched >= 1.07 J/cm>= 2.00 ft-lb/inASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C178 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 90.0 - 120 min
@Thickness 3.17 mm
1.50 - 2.00 hour
@Thickness 0.125 in
Demold
Gel Time 7.00 min
@Load 0.100 kg
7.00 min
@Load 0.221 lb
ASTM D-2971
 
Descriptive Properties
Color (cured)Translucent light brown
Mix Ratio100:100Volume
 100:88Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHAPCO173 / 317232

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.