MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo Magnum™ 344CC ABS  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

The Automotive grades of MAGNUM ABS resins offer a wide range of gloss, viscosity, impact strength and heat properties for use in numerous automotive applications. Melt flow rates from 1 to 12 g/10 min, impact strengths from 130 to 590 J/m and heat distortion temperatures from 77.C to 90.C are available. Available primarily as natural plus concentrates, MAGNUM ABS resins are used in a wide variety of automotive applications including structural instrument panels, consoles, pillars and exterior trim parts requiring painting and plating.

MAGNUM 344 CC ABS resin was specifically designed to have similar properties to MAGNUM 344 HP and to utilize the same color concentrates as MAGNUM 342EZ and 347EZ. Molders using both MAGNUM 344 CC and either 342 EZ or 347 EZ can consolidate and minimize the inventory of different color concentrates. MAGNUM 344 CC is often used in door panels, consoles and applications above the belt line where higher heat loads are experienced.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccASTM Data
Linear Mold Shrinkage 0.0050 cm/cm
Melt Flow 3.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 34.5 MPaASTM Data
Tensile Strength, Yield 44.1 MPaASTM Data
Elongation at Break 22 %ASTM Data
Tensile Modulus 2.07 GPaASTM Data
Izod Impact, Notched 2.03 J/cmASTM Data
Charpy Impact Unnotched 8.60 J/cm²ISO Data, Low Temp
 NBISO Data
Charpy Impact, Notched 0.700 J/cm²ISO Data, Low Temp
 1.50 J/cm²ISO Data
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 75.6 µm/m-°C
@Temperature 20.0 °C
ASTM data
Deflection Temperature at 0.46 MPa (66 psi) 96.1 °CUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 82.8 °CUnannealed; ASTM Data
Vicat Softening Point 111 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 344HP ABS
Trinseo Magnum™ 342EZ ABS, Medium Impact
Trinseo Magnum™ 358HP ABS, High Heat
BASF Polystyrol® 576 H Impact Grade Polystyrene (Europe)
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type

PZZDW082 / 34313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.