Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound. Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer. Uses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and Asia Information Provided by The Lubrizol Corporation |