MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 1262-80A  Polyurethane Thermoplastic Elastomer (TPU) Shielding - Stainless Steel Fiber 15% - 80 Shore A  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Shielding - Stainless Steel Fiber 15% - 80 Shore A

Comments:

  • EMI/RFI Shielding
  • ESD Protection
  • Stainless Steel Fiber
  • 80-A Durometer

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Filler Content 15 %
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 700 psiASTM D412
Elongation at Break >= 500 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 10.0 ohm-cmASTM D257
Surface Resistance <= 1e+05ASTM D257
Static Decay <= 2.0 secFTMS-4046.1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 320 - 410 °F
Mold Temperature 100 - 140 °F
Injection Pressure 10000 - 15000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MTI ThermoStran® TPU-60G Long Glass Fiber Compound
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy
Lubrizol STAT-RITE® S-1100 Static Dissipative TPU
Lubrizol LifeSciences Tecoflex® EG-93A-B40 TPU – 40% Barium Sulfate
Lubrizol LifeSciences Tecoflex® EG-93A-B20 TPU – 20% Barium Sulfate

PR5543 / 64930

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.