MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow PAPI™ 95 Polymeric MDI
Categories: Fluid; Polymer

Material Notes: PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethane diisocyanate content and a high percentage of ortho-para isomers to provide excellent flow ability and fast curing in a variety of polyurethane applications. This unique combination makes this product suitable for a full range of low and high density semi-flexible and semi-rigid foam applications that demand fast demold times for intricate parts.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.234 g/cc
Viscosity 70 cP
Molecular Weight 300 g/mol
Vapor Pressure <= 0.0000100 torr
Storage Temperature 24.0 - 38.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value 0.015% as HCl
 
Thermal PropertiesOriginal ValueComments
CTE, linear 648 µm/m-°C
@Temperature 20.0 °C
volumetric
Specific Heat Capacity 1.80 J/g-°C
Thermal Conductivity 0.000300 cal cm/sec-cm²-°C
Boiling Point 330 °C
Decomposition Temperature 230 °C
Flash Point >= 204 °CClosed Cup; ASTM D93
 
Descriptive Properties
Isocyanate Equivalent Weight132
NCO Content wt%31.8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow BETAFOAM™ 87100 MDI & PMDI Isocyanate
Dow BETAMATE™ 7200 Polyurethane Prepolymer
Dow PAPI™ 20 Polymeric MDI
Dow PAPI™ 580 N Polymeric MDI
Dow PAPI™ 94 Polymeric MDI

PDOW1400 / 30618

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.