MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Saint-Gobain CHR® A662 Aluminum Foil Backing Acrylic Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoplastic; Acrylic (PMMA)

Material Notes: CHR® A662 is manufactured from various thicknesses of aluminium foil coated with high-temperature pressure-sensitive adhesive.

Features/Benefits: CHR® A662 offers easy handling and solvent resistance. CHR® A662 is provided with a release liner. CHR® A662 can be made to meet UL, MIL-T-80B, and MIL-T-23397B Type I and Type II specifications.

Applications: CHR® A662 tape was developed as a high performance masking tape that provides area for aircraft windows during chemical stripping of old paint and for the cleaning of aircraft prior to repainting. It offers excellent protection and eliminates the danger of etching and clouding windows.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break <= 18 %<= 18 %
Tear Strength 7.89 kN/m45.0 pliInitial Tear Strength
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
ColorAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® A603 Aluminum Foil Backing Acrylic Adhesive Pressure Sensitive Tape

PSTGQZ467 / 68981

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.