MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ CA187 Thermoplastic Olefin Resin  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes:
Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent paintability, excellent surface appearance, good impact and stiffness balance

Applications: painted automotive bumper fascias

Description: Hifax CA187 medium melt flow, paintable thermoplastic elastomeric olefin resin has an excellent combination of processability and painability. It was designed primarily for painted automotive bumper fascia applications.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Linear Mold Shrinkage 0.013 cm/cmTool, Montell
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 68ISO 868
Tensile Strength, Ultimate 17.0 MPaISO R527-1
Tensile Strength, Yield 19.0 MPaISO R527-1
Elongation at Break 450 %ISO R527-1
Elongation at Yield 11 %ISO R527-1
Flexural Modulus 0.830 GPaISO 178
Izod Impact, Notched 0.220 J/cm
@Temperature -40.0 °C
ISO 180
Impact Test 25.0 J
@Temperature -30.0 °C
MAII, E at Max Load, Ductile; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°C
@Temperature -30.0 - 100 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ CA10GC Thermoplastic Polyolefin Elastomer
LyondellBasell Dexflex 980 BLK Thermoplastic Polyolefin
LyondellBasell Dexflex 810 BLK Thermoplastic Polyolefin
LyondellBasell Hifax™ CA244 Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA287AHF Thermoplastic Polyolefin Elastomer

PMO441 / 53636

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.