MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LEXAN™ Copolymer LUX9136C Polycarbonate (PC) (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and is UV stabilized providing additional weathering capability. LEXAN LUX9136C is available in diffusion colors.

Features: Low Smoke and Toxicity

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Density 1.20 g/cc0.0434 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.110 %0.110 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.13 %0.13 %ISO 62-1
Viscosity 17 cP
@Load 1.20 kg,
Temperature 300 °C
17 cP
@Load 2.65 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
0.0055 - 0.0075 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0080 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 18 g/10 min
@Load 1.20 kg,
Temperature 300 °C
18 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 54.0 MPa7830 psi50 mm/min; ASTM D638
 57.0 MPa8270 psi50 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa9140 psi50 mm/min; ISO 527
 67.0 MPa9720 psi50 mm/min; ASTM D638
Elongation at Break 73 %73 %50 mm/min; ISO 527
 80 %80 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %50 mm/min; ASTM D638
 6.0 %6.0 %50 mm/min; ISO 527
Tensile Modulus 2.30 GPa334 ksi1 mm/min; ISO 527
 2.40 GPa348 ksi50 mm/min; ASTM D638
Flexural Strength 96.0 MPa13900 psiyield, 2 mm/min; ISO 178
 103 MPa14900 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.40 GPa348 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.40 GPa348 ksi2 mm/min; ISO 178
Izod Impact Notched 100 J73.8 ft-lbASTM D256
 85.0 J
@Temperature -30.0 °C
62.7 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ASTM D4812
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²80*10*3; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBNBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 65.0 J47.9 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.78
@Frequency 1.10e+9 Hz
2.78
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Dissipation Factor 0.0056
@Frequency 1.10e+9 Hz
0.0056
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Comparative Tracking Index 175 - 250 V175 - 250 VUL 746A
Hot Wire Ignition, HWI  15 - 30 sec
@Thickness >=0.400 mm
15 - 30 sec
@Thickness >=0.0157 in
UL 746A
 >= 120 sec
@Thickness >=1.50 mm
>= 120 sec
@Thickness >=0.0591 in
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=0.400 mm
60 - 120 arcs
@Thickness >=0.0157 in
UL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  68.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 77.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
42.8 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow  70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359-2
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °C268 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 130 °C
@Thickness 3.20 mm
266 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 120 °C
@Thickness 3.20 mm
248 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 136 °C277 °FRate B/50; ASTM D1525
 139 °C282 °FRate B/50; ISO 306
 140 °C284 °FRate B/120; ISO 306
UL RTI, Electrical 130 °C266 °FUL 746B
UL RTI, Mechanical with Impact 120 °C248 °FUL 746B
UL RTI, Mechanical without Impact 130 °C266 °FUL 746B
Flammability, UL94  V-2
@Thickness >=0.400 mm
V-2
@Thickness >=0.0157 in
UL 94
 V-0
@Thickness >=1.50 mm
V-0
@Thickness >=0.0591 in
UL 94
Glow Wire Ignition Temperature  850 °C
@Thickness 1.50 mm
1560 °F
@Thickness 0.0591 in
IEC 60695-2-13
 850 °C
@Thickness 3.00 mm
1560 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 275 - 300 °C527 - 572 °F
Zone 2 270 - 295 °C518 - 563 °F
Zone 3 280 - 305 °C536 - 581 °F
Melt Temperature 280 - 305 °C536 - 581 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80401 / 288348

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.