MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Palm Labs Adhesives TURBO-LOCK SERIES 11 Anaerobic Thread Locking Compound
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: TURBO-LOCK 11 SERIES is a fast curing, BLUE, removable, medium strength, general purpose anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water, gases, oils, hydrocarbons and many chemicals. Disassembles with hand tools.

Applications:

  • Ideal for thread locking plated parts, vibration or moving components.
  • Ideal for fasteners between up to ¾” (up to 20 mm) diameters.
  • Locks and seals threaded joints-nuts, screws, and studs.
  • Meets 90% of all nut and bolt thread locking applications.
  • Meets Military specifications: MIL-S-46163

Part Numbers for this data: 11-000, 11-001, 11-010, 11-050, 11-250, 11-1000

Information provided by Palm Laboratories Adhesives

Key Words: CAS No: 923-26-2, 15625-89-5, 80-15-9 and 114-83-0
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Brookfield Viscosity 1200 cPRVT Spindle 3 @ 20 rpm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Specific Heat Capacity 0.300 J/g-°C
Thermal Conductivity 0.100 W/m-KASTM C177
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Flash Point >= 100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 hourHandling
 1.00 - 3.00 hourFunctional
 24.0 hourFull
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceBlue
Chemical Resistance100% Initial Strength RetainedAcetone at 22°C, at 500hrs
 100% Initial Strength RetainedEthanol at 22°C, at 500hrs
 100% Initial Strength RetainedMotor Oil at 125°C, at 500hrs
 100% Initial Strength RetainedGasoline at 22°C, at 500hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 500hrs
 100% Initial Strength RetainedEthanol at 22°C, at 1000hrs
 100% Initial Strength RetainedMotor Oil at 125°C, at 1000hrs
 100% Initial Strength RetainedBrake Fluid at 22°C, at 1000hrs
 80% Initial Strength RetainedWater/Glycol at 87°C, at 1000hrs
 85% Initial Strength RetainedAcetone at 22°C, at 1000hrs
 90% Initial Strength RetainedWater/Glycol at 87°C, at 500hrs
 95% Initial Strength RetainedGasoline at 22°C, at 1000hrs
CompositionMethacrylate Ester
Max Screw Size3/4" / 20mm
Torque1-4 N.mPrevail, 3/8 x 16 zinc nuts and bolts N.m, ISO 10964
 1-5 N.mPrevail, 3/8 x 16 cadmium nuts and bolts N.m, ISO 10964
 1-7 N.mBreakaway, 3/8 x 16 cadmium nuts and bolts N.m, ISO 10964
 2-7 N.mBreakaway, 3/8 x 16 zinc nuts and bolts N.m, ISO 10964
 3-7 N.mPrevail, 3/8 x 16 steel nuts and bolts N.m, ISO 10964
 8-17 N.mBreakaway, 3/8 x 16 steel nuts and bolts N.m, ISO 10964
 8-19 N.mBreakaway, M10 black oxide steel nuts and bolts N.m, ISO 10964

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPALML041 / 135195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.