MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramacast™ 583 Castable Potting Compound  (discontinued **)
Categories: Ceramic; Oxide; Magnesium Oxide; Zirconium Oxide; Potting/Casting Ceramic

Material Notes: Hydraulic setting. Castable potting compound with high dielectric strength. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils and crucibles. Supplied in powder form and are mixed with water to develop a strong hydraulic bond. Typically air set in 24 hours, then cured at 250 ºF for 2-4 hours to provide maximum electrical and mechanical properties.

Key Words: zirconia, compounds, casting, magnesium, zirconium
Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Open Porosity 7.0 %7.0 %
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 55.0 MPa7980 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm
Dielectric Strength 8.86 kV/mm225 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.00 µm/m-°C
@Temperature 20.0 °C
2.22 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 16.0 W/m-K111 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1535 °C2795 °F
 
Descriptive Properties
ColorOff White

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Repton 914 Magnesia MgO
MarkeTech Repton EXP 22 Magnesia MgO
Magnesium Oxide, MgO (Periclase)
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled
Aremco AREMCOLOX™ 502-676 Machinable Magnesium Oxide

ZCAR033 / 514

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.