MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnol® 4514 Vinyl Chloride Ethylene
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Product description: VINNOL® 4514 is an aqueous, terpolymer dispersion produced from the monomers of vinyl chloride, ethylene and a third monomer imparting amide functionality. It is used in many Engineered Fabrics, Coating, and Adhesive applications.

Properties: VINNOL® 4514 offers excellent strength, water resistance and heat sealability. The dispersion also provides good stiffness, and is very versatile in formulating. VINNOL® 4514 is a fine particle size product with excellent pigment-binding powers. Because of the vinyl chloride content, this product has superior wet and dry abrasion resistance versus conventional emulsion polymers. VINNOL® 4514 films are more hydrophobic and possess excellent alkali resistance. In addition this product is ideal for specialty coating applications where vapor barriers and fire retardancy are needed.

Application: VINNOL® 4514 can be used in a wide range of applications in the industries mentioned above, ranging from secondary binders in coatings for various masonry applications, primary binders to help add stiffness and toughness to commercial building products and various adhesive applications. In addition, VINNOL® 4514 is used in industrial automotive and HVAC filtration, as well as medical applications. Application methods include saturation, spray, foam and print bonding.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³
Solids Content 49 - 51 %49 - 51 %
pH 7.0 - 9.07.0 - 9.0
Brookfield Viscosity 25 - 150 cP25 - 150 cPLVF #2@60 rpm
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 12.0 °C53.6 °F
 
Descriptive Properties
Appearancewhite, fluid dispersion
Content<0.1%Residual monomer (vinyl acetate)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Wacker® Catalyst EM 454 Release Coating-Silicone Emulsion
Wacker Wacker® Catalyst EM 440 Release Coating-Silicone Emulsion
Wacker Wacker® Catalyst C 05 Release Coating
Wacker Vinnol® H 40/60 Vinyl Chloride Copolymer
Wacker Vinnol® H 40/43 TF Vinyl Chloride Copolymer

PWACK9669 / 205198

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.