MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kolon CGP21 Corona Metallized Packaging Film  (discontinued **)
Categories: Polymer; Film

Material Notes: Metallized Films provide excellent barrier properties and preserves contents effectively, and allow excellent printing with various optical density.

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 1.50 g/m²/day
@Thickness 0.0120 mm
0.0966 g/100 in²/day
@Thickness 0.000472 in
ASTM F1249
Oxygen Transmission Rate 1.50 cc/m²/day
@Thickness 0.0120 mm
0.0966 cc/100 in²/day
@Thickness 0.000472 in
ASTM D3985
Thickness 11.0 - 25.0 microns0.433 - 0.984 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 135 %
@Thickness 0.0120 mm
135 %
@Thickness 0.000472 in
ASTM D882
Film Elongation at Break, TD 140 %
@Thickness 0.0120 mm
140 %
@Thickness 0.000472 in
ASTM D882
Seal Strength 100 g/25 mm100 g/inAL-Adhesion
Film Tensile Strength at Break, MD 255 MPa
@Thickness 0.0120 mm
37000 psi
@Thickness 0.000472 in
ASTM D882
Film Tensile Strength at Break, TD 265 MPa
@Thickness 0.0120 mm
38400 psi
@Thickness 0.000472 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.5 %
@Thickness 0.0120 mm
4.5 %
@Thickness 0.000472 in
Heat Shrinkage; ASTM D2305
Shrinkage, TD 0.00 %
@Thickness 0.0120 mm
0.00 %
@Thickness 0.000472 in
Heat Shrinkage; ASTM D2305
 
Descriptive Properties
Optical Density2.2Kolon Test

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon CGM91 Metallized Yarn
DuPont Teijin Films Mylar® WC Polyester Film, 75 Gauge
Invista 2201U Copolymer Packaging Resin
Invista 1101R Copolymer Packaging Resin
Kolon CGM61 Non Corona Metallized Yarn

PKOKZ827 / 185370

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.