MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Novatec Novablend® 4545 PVC  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Clear Pellets

Description: Novablend® 4545 is a low-order, high impact, rigid PVC extrusion blow molding compound in pellet form. It is designed to provide excellent processing characteristics, high impact, and excellent thermal stability. Bottles produced with this compound have outstanding gloss and clarity.

Applications: Bottles made with Novablend® 4545 are suitable for use as food containers in compliance with Federal Regulation Codes. The formulation is designed to minimize odor an taste transfer to the packaged products, making this compound ideal for foods, mouthwash, edible oil, medicinals, and toiletries or cosmetics.

Information supplied by the manufacturer.

PolyOne (Avient) acquired the Novatec polymer resin product line. This grade is not a part of their current product line

Key Words: Low odor, high impact, rigid PVC compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 - 1.35 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 37.9 MPaASTM D638
Modulus of Elasticity 2.83 GPaASTM D638
Flexural Yield Strength 80.7 MPaASTM D790
Flexural Modulus 2.90 GPaASTM D790
Izod Impact, Notched 8.50 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 1601 Clear 7002 Flexible PVC
Axiall 8150 Rigid PVC, Extrusion & Molding
Colorite Polymers 2007 Rigid PVC
Colorite Polymers 2019F Rigid PVC
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12

PNV004 / 55474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.