MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Conventus Polymers Duramide™ PA66L BK Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Duramide PA66L BK is a general purpose PA66 black color with lubricant for processing aid.

Information provided by Conventus Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  62.1 MPa
@Temperature 76.7 °C
9000 psi
@Temperature 170 °F
ASTM D638
 82.7 MPa
@Temperature 22.8 °C
12000 psi
@Temperature 73.0 °F
ASTM D638
 114 MPa
@Temperature -40.0 °C
16500 psi
@Temperature -40.0 °F
ASTM D638
Tensile Strength, Yield 44.8 MPa
@Temperature 77.0 °C
6500 psi
@Temperature 171 °F
ASTM D638
Elongation at Break 60 %60 %ASTM D638
Elongation at Yield 30 %
@Temperature 76.7 °C
30 %
@Temperature 170 °F
ASTM D638
Flexural Modulus 2.83 GPa410 ksiASTM D790
Izod Impact, Notched  0.320 J/cm
@Temperature -40.0 °C
0.600 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Charpy Impact Unnotched  NB
@Temperature -34.4 °C
NB
@Temperature -30.0 °F
ISO 179/1eU
 NB
@Temperature -5.00 °C
NB
@Temperature 23.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²
@Temperature -34.4 °C
1.90 ft-lb/in²
@Temperature -30.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCONV920 / 233820

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.