MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Styrofoam™ Scoreboard Extruded Polystyrene Foam Insulation
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: STYROFOAM™ Brand Scoreboard Insulation is an extruded polystyrene foam insulation board that is scored longitudinally on 16” and 24” centers, making it easy to size to commonly used widths. STYROFOAM™ Brand Scoreboard Insulation has excellent insulating characteristics, high resistance to water and water vapor, exceptional compressive strength and long-term durability.

STYROFOAM™ Brand Scoreboard Insulation is designed for use in exterior cavity wall and foundation applications. Like all STYROFOAM™ Brand Extruded Polystyrene products, STYROFOAM™ Brand Scoreboard Insulation resists moisture to deliver a stable R-value over the long term.

This material is produced as sheets of closed-cell foam by a continuous extrusion process. Its properties will be different than expanded polystyrene beads because beads have voids between cell walls.

This former Dow product line is now a DuPont product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.30 %<= 0.30 %volume%; ASTM C272
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength >= 0.345 MPa>= 50.0 psiASTM C203
Compressive Strength >= 0.172 MPa>= 25.0 psiASTM D1621
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
35.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Insulation R Value  >= 3.8
@Thickness 19.0 mm,
Temperature 23.9 °C
>= 3.8
@Thickness 0.750 in,
Temperature 75.0 °F
ASTM C518
 >= 5.0
@Thickness 25.4 mm,
Temperature 23.9 °C
>= 5.0
@Thickness 1.00 in,
Temperature 75.0 °F
ASTM C518
 >= 7.5
@Thickness 38.1 mm,
Temperature 23.9 °C
>= 7.5
@Thickness 1.50 in,
Temperature 75.0 °F
ASTM C518
 >= 10
@Thickness 50.8 mm,
Temperature 23.9 °C
>= 10
@Thickness 2.00 in,
Temperature 75.0 °F
ASTM C518
 >= 12.5
@Thickness 63.5 mm,
Temperature 23.9 °C
>= 12.5
@Thickness 2.50 in,
Temperature 75.0 °F
ASTM C518
 >= 15
@Thickness 76.2 mm,
Temperature 23.9 °C
>= 15
@Thickness 3.00 in,
Temperature 75.0 °F
ASTM C518
Maximum Service Temperature, Air 74.0 °C165 °F
 
Descriptive Properties
Dimensional Stability2.0% Linear Change MaxASTM D2126, Thermal and Humid Aging
Flame Spread15 per ASTM E84
Smoke Developed165 per ASTM E84
Water Vapor Permeance1.5 perm MaxASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Styrofoam™ SM Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Ultra SL Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Polystyrene Rigid Foam Insulation
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)
Sekisui PIOCELAN SP-50D Moldable Polymer Foam

PDWZ00c / 209615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.