MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Algoflon® F 7 PTFE, Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Bronze Filled

Material Notes: Algoflon® F 7 is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing. It is designed for normal compression molding and in particular molding of large billets for low thickness skived tapes down to 1 mil (25 µm).

Algoflon® F 7 exhibits high bulk density, optimum isotropic behavior and very good mechanical and electrical properties.

Main features of Algoflon® F 7 are:

- Optimum mechanical properties
- Optimum isotropic properties
- Very good electrical properties
- Excellent surface finishing
- Excellent skivability

Applications: Additive; Blending

Features: Chemical Resistant

Processing
- Algoflon® F 7 is processed according to methods generally used for normal compression molding. Prior to use, the powder must be conditioned above 19°C/66°F.
- The processing involves typically two steps: preforming and sintering. Initially the powder is compacted into a preform. This is then sintered using precise sintering (heating and cooling) cycle to take the temperature above the PTFE crystalline melting point to attain the final article. The preforming pressure, dwell time at maximum sintering temperature and cooling rate are all established according to the shape and size of the final item.

Storage and Handling
- Algoflon® PTFE fine cut powders must be stored and handled carefully to achieve defect free molding. Before use the temperature of the powder must be conditioned above 19 °C / 66 °F (between 21-27 °C / 70–81 °F). Below this temperature, the powder is difficult to mold without cracks. Too high temperatures should also be avoided to prevent powder lumping and poor flow.
- Storage and handling facilities should be clean since even very small foreign particles can cause defects in finished products. Keep resin drums closed and clean. Good housekeeping and careful handling are essential.
- Each drum contains two bags liner made of polyethylene resin. The external bag liner is used only to protect the PTFE powders against external contamination. It is recommended to remove and isolate the external liner before handling and opening the internal layer which is in contact with the PTFE powders.

Safety and Toxicology
- Before using Algoflon® PTFE fine cut powders, consult the product Material Safety Data Sheet and follow all label directions and handling precautions.
- As with all PTFE materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact, wash with soap and water. In case of eye contact, flush with water immediately and seek medical help.
- Do not smoke in areas contaminated with powder, vapor or fumes.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.17 g/cc2.17 g/ccASTM D792
Bulk Density 0.410 g/cc0.0148 lb/in³ASTM D4894
Particle Size 15 µm15 µmAverage
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 44.0 MPa6380 psiASTM D4894
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 75.0 kV/mm1910 kV/inASTM D149
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
ColorWhite
FormsPowder
ProcessingCompression Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4029 / 279829

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.