MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wefapress PA 12 G Cast Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Cast

Material Notes: PA 12 G is a cast polyamide that is cast from laurin lactam without pressure. It features lower moisture absorption than the material PA 6 G. Properties: Withstands temperatures of >100°C for long periods of time, FDA-approved, High pressure resistance, High wear resistance, Conforms to EU 10/2011 (FSP variant), Excellent impact resistance.

Applications: Drive element, Components for the food industry, Sprockets, Pulleys, Gear wheels. Industries: Mechanical and plant engineering, Food industry.

Information provided by Wefapress.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccDIN 53479
Moisture Absorption <= 0.900 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
@Time 15.0 sec
DIN 53505
Ball Indentation Hardness 100 MPa
@Time 30.0 sec
DIN ISO 2039 Teil 1
Tensile Strength 70.0 MPaDIN 53455
Tensile Strength, Ultimate 70.0 MPaDIN 53455
Elongation at Break >= 55 %DIN ISO / R 527
Modulus of Elasticity 1.50 GPaDIN 53457
1% Secant Modulus 1.00 MPaEU 1935/2004 - EU 10/2011 (FSP Quality)
Charpy Impact, Notched >= 15.0 kJ/m²DIN 53457
Coefficient of Friction 0.40
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Strength 50.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CDIN ISO 11359
Specific Heat Capacity 1.70 J/g-°C
Thermal Conductivity 0.230 W/m-K
Melting Point 185 °CDTA
Maximum Service Temperature, Air 110 °CContinuous Application Temp.
Vicat Softening Point 188 °CDIN 53460
Minimum Service Temperature, Air -50.0 °C
Flammability, UL94 HB
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEFA940 / 243145

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.