MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® 3103 Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Injection molding and extrusion grade with high viscosity, UV stabilized, special grade for sheets.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³
Moisture Absorption at Equilibrium 0.15 %0.15 %50% RH
Water Absorption at Saturation 0.35 %0.35 %
 0.35 %0.35 %
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm0.0060 - 0.0080 in/inASTM D955
Melt Flow 6.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
6.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ASTM D785
Hardness, Rockwell R 118118ASTM D785
Tensile Strength, Ultimate 72.0 MPa10400 psiASTM D638
Tensile Strength, Yield 63.0 MPa9140 psi
Elongation at Break 125 %125 %ASTM D638
Elongation at Yield 6.0 %6.0 %
Tensile Modulus 2.40 GPa348 ksi
Flexural Yield Strength 86.0 MPa12500 psiat 5% strain; ASTM D790
Flexural Modulus 2.30 GPa334 ksiASTM D790
Izod Impact, Notched 9.60 J/cm
@Thickness 3.20 mm
18.0 ft-lb/in
@Thickness 0.126 in
ASTM D256
Charpy Impact Unnotched NBNB
Tensile Creep Modulus, 1 hour 2200 MPa319000 psi
Tensile Creep Modulus, 1000 hours 1900 MPa276000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm1.00e+15 ohm
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm762 kV/in
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
Arc Resistance 120 sec120 secTungsten Electrodes; ASTM D495
Comparative Tracking Index 275 V275 V
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness 3.00 mm
30 - 60 sec
@Thickness 0.118 in
UL Rating PLC 2 (30-60 sec)
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
@Thickness 1.50 mm
0.394 - 1.00 in/min
@Thickness 0.0591 in
UL Rating PLC 1 (10-25.4 mm/min.)
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°FASTM D2766
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 142 °C288 °F
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °F
Vicat Softening Point 148 °C298 °F
Glass Transition Temp, Tg 148 °C298 °F
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
Flammability, UL94 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
Oxygen Index 26 %26 %
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5861.586ASTM D542
Haze 1.0 %
@Thickness 3.20 mm
1.0 %
@Thickness 0.126 in
ASTM D1003
Transmission, Visible 88 %
@Thickness 3.20 mm
88 %
@Thickness 0.126 in
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 3103 MAS157 Polycarbonate
Techmer ES Elastoblend® PC IM
Westlake Plastics Zelux® M Machine Grade Polycarbonate
Covestro Makrolon® 1143 Polycarbonate
Covestro Makrolon® 6255 Polycarbonate

PBA440 / 26941

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.