MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Reynolds KX Flex™ 60 Fast Setting Urethane Casting Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: KX Flex™ 60 is a fast setting urethane casting elastomer that cures quickly to a flexible, highly impact resistant elastomer. KX Flex™ 60 is neutral off-white in color and easy to color using SO-Strong™, UVO™ or IGNITE™ colorants. KX Flex™ 60 has a pot life of 2.5 minutes and handling time of 20 minutes (depending on mass). With a Shore value of 60A, this rubber is used for a variety of applications including fast mold making, fast model duplication, prototyping, durable miniatures, props and special effects, or making parts that are impact resistant. Fully cured castings are flexible, tough and durable.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D-1475
Viscosity 800 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0050 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60ASTM D-2240
Tensile Strength 1800 psiASTM D-638
Elongation at Break 125 %ASTM D-638
 
Processing PropertiesOriginal ValueComments
Cure Time 20.0 minHandling
 24.0 hour
Pot Life 2.50 min
 
Descriptive Properties
ColorOff-White
Mix Ratio1A:1Bby volume or weight
Specific Volume24.1[in3/lb], ASTM D-1475

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN334 / 297035

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.