MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Jilin Xingyun Chemical 3080/3080P EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Property: Mooney viscosity high; very fast cure rate; molecular weight distribution narrow; ethylene content high; high filler ability; good blend ability with PP

Application: Resin flexibility modifier, automotive sealing strip; automotive hose; damper profiles; water-proof roll covers; plastic cement track; various extruding shaped products and sealing profiles.

Remarks: Granular product suit to blend with resin modifying flexibility. Highly effective in an improvement of filler quantity and a modification of profile appearance by blending with 3080.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %
Mooney Viscosity 65 - 75
@Temperature 125 °C
65 - 75
@Temperature 257 °F
ML 1+4
Ash <= 0.10 %<= 0.10 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 14.0 MPa>= 2030 psi
Elongation at Break >= 300 %>= 300 %
300% Modulus >= 8.00 MPa>= 1160 psi
 
Descriptive Properties
Content<10 ppmVanadium
 3-5%ENB
 65.5-71.5%Ethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJILINX010 / 317857

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.