MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Notes: ALF20 is a self-lubricating grade of nylon 66 containing PTFE and Silicone. It offers outstanding surface wear characteristics of molded parts. It is suitable for applications such as bearings and mechanical parts.

Features: Good Wear Resistance; Low Friction; Self Lubricating

Processing Method: Injection Molding

Forms: Pellets

Uses: Bearings; Machine/Mechanical parts

Injection Notes: No drying is necessary unless the material has been exposed to air for longer than 3 hours; Back Pressure: Low; Injection Pressure: High; Injection Rate: Fast

Information Provided by Teknor Apex

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 8700 psiISO 527-2
Elongation at Break 4.0 %ISO 527-2
Flexural Modulus 406000 psiISO 178
Izod Impact, Notched (ISO) 1.90 ft-lb/in²ISO 180/A
K (wear) Factor 12.0 x 10-10 in³-min/ft-lb-hrASTM D3702
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) >= 392 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 203 °FISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 518 - 554 °F
Middle Barrel Temperature 518 - 554 °F
Front Barrel Temperature 518 - 554 °F
Melt Temperature 518 - 554 °FProcessing Temp
Mold Temperature 68.0 - 104 °F
Drying Temperature 176 °F
Dry Time 2 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
UBE UPIMOL® S High Heat Polyimide Shape
Techmer ES HiFill FR® PA4/6 FR HS
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled
Celanese Nilit FRIANYL A63 N-SG5 Nylon 6.6 for injection molding, 5% mineral filled

PTEKNO428 / 128605

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.