Hostacom G3 N13 C1 Black is a 30% glass fiber reinforced polypropylene. This product is intended for injection molding. It is optimized for applications where excellent stiffness and impact resistance are required over a wide temperature range. The product is available as a customized color matched, pellet form. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Asia-Pacific Processing Method: Injection Molding Attribute: Good Dimensional Stability; Good Impact Resistance; Good Stiffness Information provided by LyondellBasell. |