MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 246M Black 21 N PA 66, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: TECHNYL® A 246M Black 21 N is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in black color.

Key Properties: Very high impact even at low temperature

Benefits: This product offers an excellent notched impact resistance, even at low temperature.

Applications: The product is suitable for all kind of applications ( automotive, sport, leisure,…) that required a high level of impact resistance.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 1.05 %
@Time 86400 sec
ISO 62
Viscosity 13 cP
@Shear Rate 10000 1/s,
Temperature 290 °C
 20 cP
@Shear Rate 10000 1/s,
Temperature 280 °C
 22 cP
@Shear Rate 10000 1/s,
Temperature 270 °C
 32 cP
@Shear Rate 100 1/s,
Temperature 290 °C
 50 cP
@Shear Rate 100 1/s,
Temperature 280 °C
 122 cP
@Shear Rate 100 1/s,
Temperature 270 °C
Linear Mold Shrinkage 0.010 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.019 cm/cm
Linear Mold Shrinkage, Transverse 0.019 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.0 MPaISO 527 Type 1A
Tensile Strength, Yield 47.0 MPaISO 527 Type 1A
 50.0 MPaASTM D635
Tensile Stress at Strain 30.0 MPa
@Strain 2 %
 38.0 MPa
@Strain 4 %
 45.0 MPa
@Strain 20 %
Elongation at Break 80 %ISO 527 Type 1A
Elongation at Yield 20 %ISO 527 Type 1A
Tensile Modulus 1900 MPaISO 527 Type 1A
Flexural Strength 70.0 MPaISO 178
Flexural Modulus 1800 MPaISO 178
Izod Impact, Unnotched 10.2 J/mASTM D256
Izod Impact, Notched (ISO) 22.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 16.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 97.0 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohmIEC 60093
Dielectric Constant 3.2IEC 60250
Dielectric Strength 30.0 kV/mmIEC 60243
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 450 VSol B; IEC 60112
 575 VSol A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °CASTM D648
 65.0 °CISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
ISO 1210
Oxygen Index 24.5 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 - 280 °CCompression zone
 270 - 290 °CMixing zone
Feed Temperature 250 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY844 / 218572

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.