MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 1.6 %
@Thickness 3.18 mm
1.6 %
@Thickness 0.125 in
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.011 - 0.013 cm/cm0.011 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 77.9 MPa11300 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 60 %60 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.55 GPa370 ksiASTM D638
Flexural Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.52 GPa365 ksiASTM D790
Izod Impact, Notched 0.530 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 215 °C419 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
@Thickness 3.18 mm
140 °F
@Thickness 0.125 in
Unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Mold Temperature 48.9 - 93.3 °C120 - 200 °F
Drying Temperature 82.2 °C180 °F
Dry Time 4.00 hour4.00 hour
 
Descriptive Properties
AppearanceNatural Color
FeaturesGeneral Purpose
 Lubricated
FormsPellets
Generic MaterialNylon 6 Alloy
Generic NamePolyamide 6 Alloy (Nylon 6 Alloy)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ BA50-100 Blow Molding Resin
Avient Nymax™ 600 A Natural Polyamide 6 Alloy (Nylon 6 Alloy)
Avient Nymax™ 600 A HS Natural A Polyamide 6 Alloy (Nylon 6 Alloy)
Avient Nymax™ 600 Zip 0 Black 13 Polyamide 6 Alloy (Nylon 6 Alloy)

PH0POL0943 / 145512

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.