MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sinotek Materials R20 P Carbon Rod for Dry Battery
Categories: Carbon; Graphite

Material Notes: We offer carbon rods for dry batteries in 11 regular sizes, including R03, R1, R6,R10, R12,R14, R20, R25, R40, S4, AR40 etc.; In 3 grades, 1st-class, 2nd-class , 3rd-class; And 5 types in waterproofness, impregnation, S, O, C, P, PS; Totaling more than hundred models.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength >= 32.0 MPa>= 4640 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.0040 ohm-cm<= 0.0040 ohm-cm
 
Descriptive Properties
Air Permeability (4kg/cm2, ml/min)0
Filling %>85
Hole Content %20-25
Impregnation %>8.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Graphite, Carbon, C
Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Sinotek Materials 3rd Class Carbon Rod for Dry Battery
BACT Metal-Dylyn® Diamond-Like Nanocomposite Coating
BACT Dylyn® Diamond-Like Nanocomposite Coating

CSINOT82 / 2139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.