MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

DuPont Mobility and Materials MEGUM™ 3270 BG Primer
Categories: Fluid

Material Notes: Colored solvent-based primer, used in combination with MEGUM or THIXON™ cover coats.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 - 0.960 g/cc0.0332 - 0.0347 lb/in³ISO 845
 1.83 g/cc0.0661 lb/in³Dry Film
Solids Content 23 - 26 %23 - 26 %
Volatile Organic Compounds (VOC) Content 690 g/l690 g/l
Viscosity 120 - 250 cP120 - 250 cP
Brookfield Viscosity 12 - 25 cP12 - 25 cP
 25 cP25 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 17.0 °C62.6 °FASTM D 92
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 °C
@Time >=299 sec
320 °F
@Time >=0.0830 hour
Oven pre-bake
Dry Time 0.500 hour0.500 hourApplication technique
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
ColorBlue
CompatibilityMetals
 Nitrile Rubber
 Rubber
Dilution, parts diluent0.1 - 0.3dipping
 0.4 - 1spraying
 undilutedbrushing
PolymerPrimer
Recommended application film thickness5 - 15 µm
Regional AvailabilityEurope
 Near East/Africa
Solventketones MIBK MIBK/xylene (1:1)
Theoretical coverage (m²/L)12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4834f / 290951

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.