MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Trigonox 44K Acetylacetone peroxide and tert-butyl peroxybenzoate, in solvent mixture
Categories: Other Engineering Material

Material Notes: Trigonox 44K is a highly reactive & efficient cure system for ambient to elevated temperature curing of promoted unsaturated polyester & acrylic modified thermoset resins. Phthalate-free initiator blend used to drive fast and complete cure where fast exotherm can be accepted.

CAS number: 37187-22-7; 614-45-9

EINECS/ELINCS No: 253 253-384-9; 210-382-2

Applications: Trigonox 44K is a phthalate-free blended initiator used for the curing of unsaturated polyester and acrylic thermoset resins at ambient conditions in conjunction with metal salts. Trigonox 44K provides for effective through-cure and lower residual monomer contents in applications such as panels and laminates. Additional end-use information is available in various application guides or directly from Nouryon representative.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³
Storage Temperature -10.0 - 30.0 °C14.0 - 86.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 60.0 °C140 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Content3.41-3.63 %Total active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1129 / 286652

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.