MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems RenShape® SL 7820 Stereolithography Plastic
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appearance. It offers a large working envelope of physical properties, high elongation and impact strength suitable for building concept models, and functional prototype parts.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
@Temperature 25.0 °C
Liquid
 1.16 g/cc
@Temperature 25.0 °C
Solid
Viscosity 210 cP
@Temperature 30.0 °C
 240 cP
@Temperature 28.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Tensile Strength 36.0 - 51.0 MPaASTM D638
Elongation at Break 8 - 18 %ASTM D638
Tensile Modulus 1900 - 2400 MPaASTM D638
Flexural Strength 59.0 - 80.0 MPaASTM D790
Flexural Modulus 2000 - 2400 MPaASTM D790
Izod Impact, Notched 42.0 - 48.0 J/mASTM D256
Penetration 4.5mils penetration depth
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °Cbelow Tg; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.1 °CASTM D648
Glass Transition Temp, Tg 62.0 °CDMA, E"
 
Descriptive Properties
AppearanceDark brown to blackcured
 Whiteliquid
Critical Exposure (Ec)10 mJ/cm²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
DSM Somos® WaterShed® 11110 Water-resistant resin for stereolithography
DSM Somos® WaterShed® 11120 Water-resistant resin for stereolithography

PHURE990 / 176026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.