MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals SURPASS® HPs667-AB sHDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes:

Homopolymer

Features:

  • Superior barrier properties
  • Very high stiffness
  • Low gel

Additives:

  • Processing antioxidant

Applications:

  • Moisture barrier films
  • Co-extrusion
  • Dry food packaging
  • Cast film
  • Extrusion lamination

Film properties are measured on a cast film. Processing conditions 350 lb/hr, 30" die and a 25 mil die gap.

United States: SURPASS HPs667-AB resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.2, and may thus be used in the United States as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.968 g/ccASTM D 792
Water Vapor Transmission 1.20 g/m²/day
@Temperature 38.0 °C
100% RH; ASTM F 1249
Oxygen Transmission Rate 700 cc/m²/day
@Temperature 23.0 °C
0% RH; ASTM D 3985
Thickness 50.0 microns
Melt Index of Compound 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 25.0 MPaASTM D 882
Film Tensile Strength at Yield, TD 24.0 MPaASTM D 882
Elmendorf Tear Strength MD 40 gASTM D 1922
Elmendorf Tear Strength TD 70 gASTM D 1922
1% Secant Modulus, MD 1050 MPaASTM D 882
1% Secant Modulus, TD 1250 MPaASTM D 882
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)15NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NOVA Chemicals NOVAPOL® LF-0222-F LDPE Clarity Film Resin
NOVA Chemicals SURPASS® CCs757-A sHDPE Injection Molding Resin
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin
NOVA Chemicals SCLAIR® 2807CC-NS HDPE Injection Molding Resin
NOVA Chemicals SCLAIR® 2807CC HDPE Injection Molding Resin

PNOVB094 / 194702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.