The Pyro-Bloc Y and Y2 modules are manufactured from a high purity blend of raw materials which are used to produce ZR Grade (alumina-zirconia-silica) ceramic fibers. The modules utilize a specially designed 316 stainless steel internal support system and industry standard Pyro-Bloc stud system. In addition, it has no hot face, cold face, or side constrictions which permit maximum module-to-module compression during installation. The modules use the proven center-fire, one-step weld system which eliminates the need for pre-laid out stud patterns. Features: Monolithic, edge-grained ceramic fiber module Available in uncompressed densities from 8 - 15 pcf (128-240 kg/m3 ) One-shot center-fired stud Extremely fast, efficient installation High density fiber resists mechanical abuse Applications: Annealing furnaces Heat treating furnaces Process heaters Reformers Ethylene furnaces Forge furnaces Steam flood units Homogenizing furnaces IncineratorsInformation provided by Thermal Ceramics Data has not been recently verified. Please contact manufacturer for current information. |